Steve Harrison
kiln 3 |
|
At right: interior of the front chamber The kiln is fired over two days. Steve says he is “not a great believer in very hot firings” and fires to a temperature between Orton cones 10 and 11.
Materials for this kiln: mainly secondhand dense fire bricks, although Steve has experimented with making his own firebricks.
|
Click on any image below to reach an enlargement |
Bagwall in the second chamber |
Above: exit flues for second chamber have been adjusted with bits of shelf
|